The stabilized modified liquid is injected into the wood cell wall through a vacuum pressure equipment, and then cured at high temperature. After the stabilized modified liquid, the weight of the wood can be increased by 1-3 times, the hardness can be increased by 1-4 times, and the water resistance can be increased. It can be increased by 5-10 times, the pressure resistance can be increased by 3-8 times, and the corrosion resistance can be increased by more than 8 times. The index of cracking and deformation of the improved wood can reach 0.3 mm/square by the high and low temperature cold and hot immersion cooking test method. meters below. The original lumen fiber strength, cell wall fiber strength, and longitudinal fibers of the wood can be effectively improved, thereby completely preventing and reducing the warpage, deformation and cracking of the wood caused by natural climate changes.